Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|---|---|---|
Surface tension Metallizedside | ASTMD2578 | 56 mN/m | |
ASTMD2578 | 56 mN/m | ||
Shrinkage rate | ASTMD1204 | 2.5 % | |
ASTMD1204 | 2.5 % | ||
ASTMD1204 | 0.40 % | ||
ASTMD1204 | 0.40 % |
optical performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Optical Density | 内部方法 | -2.4到7.6 % | |
内部方法 | -2.4到7.6 % |
film | Test Condition | Test Method | Test Result |
---|---|---|---|
Film thickness - tested | 1012 µm | ||
Available film thickness | 10,12µm | ||
tensile strength | ASTMD882 | 206 MPa | |
elongation | ASTMD882 | 90 % | |
oxygen permeability | ASTMD3985 | 0.700 cm³/m²/24hr | |
ASTMD3985 | 0.800 cm³/m²/24hr | ||
Water vapor permeability | ASTMF1249 | 0.40 g/m²/24hr | |
ASTMF1249 | 0.50 g/m²/24hr | ||
usage | 内部方法 | 71.4 m²/kg | |
内部方法 | 59.5 m²/kg | ||
tensile strength | ASTMD882 | 206 MPa | |
ASTMD882 | 216 MPa | ||
ASTMD882 | 216 MPa | ||
elongation | ASTMD882 | 100 % | |
ASTMD882 | 100 % | ||
ASTMD882 | 90 % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.