TPE ATPR 2000 70A

0

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
densityASTMD7920.948到1.10 g/cm³
melt mass-flow rateASTMD12388.0 g/10min
hardnessTest ConditionTest MethodTest Result
Shore AASTMD224070
Mechanical propertiesTest ConditionTest MethodTest Result
Tensile modulusASTMD4121.59 MPa
ASTMD1044125 mg
elastomerTest ConditionTest MethodTest Result
tensile strengthYieldASTMD4126.76 MPa
elongationBreakASTMD412700 %
tear strengthASTMD62427.1 kN/m
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.