ABS/PBT NOVALLOY B  BM5544

716

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
Shrinkage rateASTM D9550.20 - 0.40 %
flammabilityTest ConditionTest MethodTest Result
UL flame retardant ratingUL 94V-1
UL flame retardant ratingUL 94V-0
Mechanical propertiesTest ConditionTest MethodTest Result
tensile strength ISO 527-2130 Mpa
Flexural modulusISO 17811000 Mpa
bending strengthISO 178205 Mpa
Electrical performanceTest ConditionTest MethodTest Result
Surface Resistivity内部方法4.0E+2 ohms
Volume resistivity内部方法1.0E+2 ohms·cm
injectionTest ConditionTest MethodTest Result
drying temperature80 to 120 °C
drying time3.0 to 5.0 hr
Temperature at the rear of the barrel190 to 230 °C
Temperature in the middle of the barrel220 to 240 °C
Temperature at the front of the material cylinder240 to 250 °C
Spray nozzle temperature230 to 250 °C
Temperature60 to 80 °C
Back pressure5.00 to 20.0 Mpa
screw speed50 to 90 rpm
Thermal performanceTest ConditionTest MethodTest Result
Heat distortion temperatureISO 75-2/A155 °C
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.