Technical Data Sheet
Basic performance | Test Condition | Test Method | Test Result |
---|---|---|---|
density | ISO 1183 | 1050 kg/m | |
Melt Mass-Flow Rate | ISO 1133 | 18.0 cm |
Mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Tensile Stress (Yield) | ISO 527-1,-2 | 2.5 % | |
fracture strain | ISO 527-1,-2 | 0.00 % | |
Charpy notch impact strength | ISO 179/1eA | 19.0 KJ/m | |
ISO 179/1eA | 10.0 KJ/m | ||
Charpy impact strength | ISO 179/1eU | 80.0 KJ/m | |
ISO 179/1eU | 80.0 KJ/m | ||
Tensile modulus | ISO 527-1,-2 | 2400 MPa | |
yield stress | ISO 527-1,-2 | 47.0 MPa |
Electrical performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Volume resistivity | IEC 60093 | 1E+13 ohm.m | |
Relative Permittivity | IEC 60250 | 3.10 | |
Dielectric loss factor | IEC 60250 | 0.0080 | |
electric strength | IEC 60243-1 | 32 KV/mm | |
Relative Permittivity | IEC 60250 | 2.90 | |
Dielectric loss factor | IEC 60250 | 0.0060 |
Thermal performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Heat Deflection Temperature | ISO 75-1,-2 | 100 ℃ | |
ISO 75-1,-2 | 96.0 ℃ | ||
vicat | ISO 306 | 97.0 ℃ | |
Coefficient of Linear Thermal Expansion | ISO 11359-1,-2 | 0.000090 cm/cm℃ |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.