  • Properties:
    Filler
    glass beads
    20%
    filler by weight

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
Shrinkage rateASTM D9551.2to1.6 %
densityASTM D7921.43 g/cm³
melt mass-flow rateASTM D123834 g/10min
ash contentASTM D258418to22 %
Impact resistanceTest ConditionTest MethodTest Result
Charpy Notched Impact StrengthISO 1793.5 kJ/m²
Impact strength of simply supported beam without notchASTM D25625.0 kJ/m²
Mechanical propertiesTest ConditionTest MethodTest Result
Tensile modulusASTM D6383300 MPa
tensile strength ASTM D63860.0 MPa
elongationASTM D6384.0 %
Thermal performanceTest ConditionTest MethodTest Result
Heat distortion temperatureASTM D648180 °C
Heat distortion temperatureASTM D64875.0 °C
melting temperatureASTM D2117225 °C
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.