Technical Data Sheet
物理性能 | Test Condition | Test Method | Test Result |
---|
收缩率 | TD | ISO294-4 | 1.2 % |
收缩率 | MD | ISO294-4 | 1.2 % |
吸水率 | 饱和,23°C,2.00mm | ISO62 | 3.8 % |
吸水率 | 平衡,23°C,2.00mm,50%RH | ISO62 | 1.7 % |
热性能 | Test Condition | Test Method | Test Result |
---|
热变形温度 | 0.45MPa,未退火 | ISO75-2/B | 140 °C |
热变形温度 | 1.8MPa,未退火 | ISO75-2/A | 50.0 °C |
玻璃转化温度2 | | ISO11357-2 | 60.0 °C |
熔融温度 | | ISO11357-3 | 223 °C |
可燃性 | Test Condition | Test Method | Test Result |
---|
燃烧速率3 | 1.00mm | ISO3795 | <100 mm/min |
FMVSS可燃性 | | FMVSS302 | B |
机械性能 | Test Condition | Test Method | Test Result |
---|
拉伸模量 | | ISO527-2 | 2400 Mpa |
拉伸应力 | 屈服 | ISO527-2 | 68.0 Mpa |
拉伸应变 | 屈服 | ISO527-2 | 4.5 % |
冲击性能 | Test Condition | Test Method | Test Result |
---|
简支梁无缺口冲击强度 | 23°C | ISO179/1eU | 34 kJ/m² |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.