Product Description
| Typical Applications: | Industrial applications | home appliance components | applications in the automotive field | automotive interior parts |
| Properties: | Filler | ADDIPLAST | French ADDIPLAST |
Certificates
No Data...
Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Charpy Notched Impact Strength | ISO 179/1eA | 4.0 | kJ/m² | |
| Impact strength of simply supported beam without notch | ISO 179/1eU | 无断裂 | ||
| Impact strength of cantilever beam gap | ISO 180/1A | 4.0 | kJ/m² | |
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| tensile strength | Yield | ISO 527-2 | 21.0 | MPa |
| Bending modulus | ISO 178 | 2700 | MPa | |
| tensile strength | Break | ISO 527-2 | 19.0 | MPa |
| Tensile strain | Break | ISO 527-2 | >100 | % |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Hot deformation temperature | 1.8MPa,Unannealed | ISO 75-2/Af | 67.0 | °C |
| Vicat softening temperature | ISO 306/A50 | 153 | °C | |
| Melting temperature | ISO 3146 | 165to168 | °C | |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| density | ISO 1183/A | 1.23 | g/cm³ | |
| melt mass-flow rate | 230°C/2.16kg | ISO 1133 | 18 | g/10min |
| Electrical performance | Test Condition | Test Method | Test Result | Test Unit |
| Volume resistivity | IEC 60093 | >1.0E+15 | ohms·cm | |
| Compared to the anti leakage trace index | SolutionA | IEC 60112 | PLC 0 | |
| Surface resistivity | IEC 60093 | 1E+14 | ohms | |
| hardness | Test Condition | Test Method | Test Result | Test Unit |
| Shore hardness | ShoreD | ISO 868 | 75 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.