film | Test Condition | Test Method | Test Result |
---|---|---|---|
Film thickness - tested | 51 µm | ||
tensile strength | Yield | ASTMD882 | 31.0 MPa |
Break | ASTMD882 | 112 MPa | |
elongation | Break | ASTMD882 | 380 % |
Elmondov tear strength MD | ASTMD1922 | 130 g |
Thermal performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Crystallization peak temperature | ASTMD3418 | 218到220 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.