Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|---|---|---|
VOCContent | 0.30 % | ||
0.900到2.00 mm | |||
density | ASTMD3575 | 0.0240 g/cm³ | |
VOCContent | 7.5 % |
Supplementary Information | Test Condition | Test Method | Test Result |
---|---|---|---|
Puncture | ASTMD3763 | 198 N | |
Tear strength - atMaximmLoad | ASTMD3575 | 1.8 kN/m |
Mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
tensile strength | Break | ASTMD3575 | 0.356 MPa |
bending strength | ASTMC203 | 0.317 MPa | |
ASTMC203 | 0.352 MPa | ||
compressive strength | ASTMD3575 | 0.144 MPa | |
ASTMD3575 | 0.168 MPa | ||
ASTMD3575 | 0.230 MPa | ||
ASTMD3575 | 0.490 MPa | ||
Bending Strain | ASTMC203 | 11 % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.