Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|
melt mass-flow rate | | ASTMD1238 | 65 g/10min |
melt mass-flow rate | | ASTMD1238 | 1300 g/10min |
Content of comonomer | | 内部方法 | 20.0 % |
other | Test Condition | Test Method | Test Result |
---|
characteristic | | | 高熔指 高AA含量 |
purpose | | | 高档服装衣领的涂覆 水性溶剂 高温火焰喷涂 环保降解材料 |
Basic performance | Test Condition | Test Method | Test Result |
---|
melt mass-flow rate | | ASTM D-1238 | 1300 g/10min |
melt mass-flow rate | | ISO 1133 | 1300 g/10min |
Monomer content | | Internal Method | % |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
Tensile modulus | | ASTM D-638 | 22.1 MPa |
Tensile modulus | | ISO 527-2 | 22.1 MPa |
tensile strength | | ASTM D-638 | 6.21 MPa |
tensile strength | | ISO 527-2 | 6.21 MPa |
elongation at break | | ASTM D-638 | 350 % |
elongation at break | | ISO 527-2 | 350 % |
Tensile modulus | | ASTMD638 | 22.1 Mpa |
tensile strength | | ASTMD638 | 6.21 Mpa |
elongation | | ASTMD638 | 350 % |
Thermal performance | Test Condition | Test Method | Test Result |
---|
melting temperature | | Internal Method | 75 ℃ |
vicat | | ASTMD1525 | 40.0 °C |
melting temperature | | 内部方法 | 75.0 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.