Technical Data Sheet
物理性能 | Test Condition | Test Method | Test Result |
---|
熔体质量流动速率 | 190°C/2.16kg | ASTMD1238 | 10 g/10min |
收缩率 | MD:2.00mm | ASTMD955 | 0.40 % |
吸水率 | 平衡,23°C,65%RH | ASTMD570 | 0.56 % |
热性能 | Test Condition | Test Method | Test Result |
---|
脆化温度 | | ASTMD746 | -65.0 °C |
维卡软化温度 | | ASTMD1525 | 89.0 °C |
熔融温度 | | DSC | 180 °C |
线性热膨胀系数 | MD | ASTMD696 | 2E-04 cm/cm/°C |
可燃性 | Test Condition | Test Method | Test Result |
---|
UL阻燃等级 | | UL94 | HB |
机械性能 | Test Condition | Test Method | Test Result |
---|
抗张强度 | 屈服 | ASTMD638 | 14.0 Mpa |
伸长率 | 断裂 | ASTMD638 | 820 % |
弯曲模量 | | ASTMD790 | 23.0 Mpa |
压缩模量 | | ASTMD695 | 2.40 Mpa |
泰伯耐磨性 | 1000Cycles | ASTMD1044 | 20.0 mg |
电气性能 | Test Condition | Test Method | Test Result |
---|
体积电阻率 | | ASTMD257 | 1E+12 ohms·cm |
介电强度 | | ASTMD149 | 20 KV/mm |
硬度 | Test Condition | Test Method | Test Result |
---|
肖氏硬度 | 邵氏D | ASTMD2240 | 31 |
弹性体 | Test Condition | Test Method | Test Result |
---|
拉伸应力 | 50%应变 | ASTMD412 | 3.40 Mpa |
撕裂强度 | | ASTMD624 | 76.0 kN/m |
压缩永久变形 | | ASTMD395 | 49 % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.