TPV Alloy Elastoprene 75A-4000

0

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
densityASTMD7920.950 g/cm³
hardnessTest ConditionTest MethodTest Result
ASTMD224075
ASTMD224073
Supplementary InformationTest ConditionTest MethodTest Result
OzoneResistanceASTMD1149Excellent
elastomerTest ConditionTest MethodTest Result
tear strengthASTMD62440.0 kN/m
compression setASTMD39530 %
compression setASTMD39552 %
Tensile stressASTMD4125.00 MPa
tensile strengthASTMD4126.00 MPa
elongationASTMD412520 %
agingTest ConditionTest MethodTest Result
Change rate of ultimate elongation in airASTMD573-6.0 %
The rate of change in hardness of an air hardness testerASTMD5734.0
Change rate of tensile strength in airASTMD573-11 %
Thermal performanceTest ConditionTest MethodTest Result
brittle temperatureASTMD746-70.0 °C
melting temperature159 °C
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.