Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|---|---|---|
density | ASTM D1505 | 1.40 g/cm³ | |
Shrinkage rate | 内部方法 | 1.0 % | |
内部方法 | 1.0 % | ||
内部方法 | 0.40 % | ||
内部方法 | 0.40 % |
optical performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Haze ratio | ASTM D1003 | 4.0 % | |
ASTM D1003 | 3.8 % | ||
gloss | ASTM D523 | 170 | |
ASTM D523 | 171 | ||
transmissivity | ASTM D1003 | 89.0 % | |
ASTM D1003 | 89.0 % |
Mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
coefficient of friction | ASTM D1894 | 0.30 | |
ASTM D1894 | 0.40 | ||
ASTM D1894 | 0.30 | ||
ASTM D1894 | 0.40 |
film | Test Condition | Test Method | Test Result |
---|---|---|---|
tensile strength | ASTM D882 | 214 MPa | |
ASTM D882 | 207 MPa | ||
ASTM D882 | 234 MPa | ||
ASTM D882 | 228 MPa | ||
elongation | ASTM D882 | 160 % | |
ASTM D882 | 160 % | ||
ASTM D882 | 130 % | ||
ASTM D882 | 140 % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.