POM Copolymer Hoegerin® 511 HP-T H?glmeier Polymer-Tech GmbH & Co. KG
Product Description
Certificates(0)
Datasheet
Product Description
Certificates
No Data...
Technical Data Sheet
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| Tensile modulus | ISO 527-2 | 3250 | MPa | |
| tensile strength | Break | ISO 527-2 | 67.0 | MPa |
| -- | ISO 527-2 | 71.0 | MPa | |
| Tensile strain | Break | ISO 527-2 | 17 | % |
| thermal performance | Test Condition | Test Method | Test Result | Test Unit |
| Crystallization peak temperature | DSC | ISO 3146 | 175 | °C |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| Melt Volume Flow Rate (MVR) | 190°C/21.6kg | ISO 1133 | 12.5 | cm³/10min |
| ash content | DIN EN60 | <0.10 | % | |
| density | 23°C | DIN 53479 | 1.42 | g/cm³ |
| melt mass-flow rate | 190°C/21.6kg | ISO 1133 | 14 | g/10min |
| hardness | Test Condition | Test Method | Test Result | Test Unit |
| Shore hardness | ShoreD | 81 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.