Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|
density | | ASTMD1505 | 1.40 g/cm³ |
optical performance | Test Condition | Test Method | Test Result |
---|
transmissivity | | ASTMD1003 | 86.0 % |
Haze ratio | | ASTMD1003 | 11 % |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
| Itself - Static | ASTMD1894 | 0.40 |
film | Test Condition | Test Method | Test Result |
---|
tensile strength | | ASTMD882 | 193 MPa |
tensile strength | | ASTMD882 | 228 MPa |
elongation | | ASTMD882 | 150 % |
elongation | | ASTMD882 | 110 % |
Film thickness - tested | | | 51 µm |
tensile strength | | ASTMD882 | 100 MPa |
tensile strength | | ASTMD882 | 103 MPa |
Thermal performance | Test Condition | Test Method | Test Result |
---|
melting temperature | | | 260 °C |
| | ASTMD696 | 1.8E-05 cm/cm/°C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.