Technical Data Sheet
物理性能 | Test Condition | Test Method | Test Result |
---|
密度 | | ASTMD792 | 1.20 g/cm³ |
收缩率 | MD:3.20mm | ASTMD955 | 0.20to0.60 % |
热性能 | Test Condition | Test Method | Test Result |
---|
热变形温度 | 0.45MPa,未退火 | ASTMD648 | 73.0 °C |
热变形温度 | 1.8MPa,未退火 | ASTMD648 | 65.0 °C |
光学性能 | Test Condition | Test Method | Test Result |
---|
透射率 | 总计 | ASTMD1003 | 91.0 % |
透射率 | Regular | ASTMD1003 | 89.0 % |
雾度 | | ASTMD1003 | 0.30 % |
机械性能 | Test Condition | Test Method | Test Result |
---|
拉伸应变 | 断裂,23°C | ISO527-2 | 200 % |
弯曲模量 | 23°C | ASTMD790 | 2000 Mpa |
弯曲模量 | 23°C | ISO178 | 1850 Mpa |
弯曲应力 | 23°C | ISO178 | 65.0 Mpa |
弯曲强度 | 屈服,23°C | ASTMD790 | 69.0 Mpa |
拉伸模量 | 23°C | ISO527-2 | 1800 Mpa |
抗张强度 | 屈服,23°C | ASTMD638 | 47.0 Mpa |
拉伸应力 | 屈服,23°C | ISO527-2 | 47.0 Mpa |
抗张强度 | 断裂,23°C | ASTMD638 | 51.0 Mpa |
拉伸应力 | 断裂,23°C | ISO527-2 | 46.0 Mpa |
伸长率 | 屈服,23°C | ASTMD638 | 5.0 % |
拉伸应变 | 屈服,23°C | ISO527-2 | 4.0 % |
伸长率 | 断裂,23°C | ASTMD638 | 320 % |
硬度 | Test Condition | Test Method | Test Result |
---|
洛氏硬度 | R计秤,23°C | ASTMD785 | 103 |
冲击性能 | Test Condition | Test Method | Test Result |
---|
悬壁梁缺口冲击强度 | -40°C | ASTMD256 | 40 J/m |
悬壁梁缺口冲击强度 | 23°C | ASTMD256 | 80 J/m |
悬壁梁缺口冲击强度 | -40°C | ISO180 | 4.8 kJ/m² |
悬壁梁缺口冲击强度 | 23°C | ISO180 | 7.8 kJ/m² |
悬壁梁缺口冲击强度 | -40°C | ASTMD4218 | NoBreak |
悬壁梁缺口冲击强度 | 23°C | ASTMD4218 | NoBreak |
装有测量仪表的落镖冲击 | -40°C,EnergyatPeakLoad | ASTMD3763 | 48.0 J |
装有测量仪表的落镖冲击 | 23°C,EnergyatPeakLoad | ASTMD3763 | 42.0 J |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.