PUR-Ester Andur 900-AP USA Anderson Development
Product Description
Certificates(0)
Datasheet
Product Description
Certificates
No Data...
Technical Data Sheet
| elastomer | Test Condition | Test Method | Test Result | Test Unit |
|---|---|---|---|---|
| tensile strength | 100%Strain | ASTM D412 | 9.63 | MPa |
| 200%Strain | ASTM D412 | 14.8 | MPa | |
| 300%Strain | ASTM D412 | 25.9 | MPa | |
| Permanent compression deformation | ASTM D395 | 28 | % | |
| mechanical properties | Test Condition | Test Method | Test Result | Test Unit |
| tensile strength | Yield | ASTM D638 | 41.8 | MPa |
| elongation | Yield | ASTM D638 | 550 | % |
| thermosetting | Test Condition | Test Method | Test Result | Test Unit |
| storage stability | 70°C | 4.0to6.0 | min | |
| Thermosetting mixed viscosity | 70°C | ASTM D2393 | 2660 | cP |
| stripping time | 100°C | 180 | min | |
| Physical properties | Test Condition | Test Method | Test Result | Test Unit |
| Apparent density | ASTM D1895 | 1.14 | g/cm³ | |
| Shrinkage rate | MD | ASTM D955 | 1.6 | % |
| hardness | Test Condition | Test Method | Test Result | Test Unit |
| Shore hardness | ShoreA | ASTM D2240 | 90 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.