PP Alloy Propafilm™ RDU85

0

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
Shrinkage rate内部方法4.0 %
Shrinkage rate内部方法7.0 %
Shrinkage rate内部方法1.0 %
optical performance Test ConditionTest MethodTest Result
glossASTMD2457100
Haze ratioASTMD10032.0到3.0 %
Mechanical propertiesTest ConditionTest MethodTest Result
ASTMD18940.20到0.30
ASTMD18940.20到0.30
filmTest ConditionTest MethodTest Result
Sealing emphasis内部方法0.15 N/mm
Sealing emphasis内部方法0.15 N/mm
内部方法104到146 °C
内部方法85.0到146 °C
oxygen permeabilityASTMF19270.16 cm³·mm/m²/atm/24hr
oxygen permeabilityASTMF19270.16 cm³·mm/m²/atm/24hr
Water vapor permeabilityASTMF17704.0 g/m²/24hr
usage内部方法51.0 m²/kg
Film thickness - tested2200 µm
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.