plas
Log In

PEEK Pyramid™ PEEK KD2450-NT Polymics, Ltd.

0
  • Properties:
    Filler ceramic fiber filler 30% filler by weight
  • Compare

Technical Data Sheet

impact performanceTest ConditionTest MethodTest Result
Impact strength of cantilever beam gap3.18mmASTM D25653 J/m
mechanical propertiesTest ConditionTest MethodTest Result
Tensile modulusASTM D6384140 MPa
tensile strengthBreakASTM D63879.3 MPa
elongationBreakASTM D638>10 %
Bending modulusASTM D7904140 MPa
bending strengthYieldASTM D790152 MPa
thermal performanceTest ConditionTest MethodTest Result
Glass transition temperatureDSC143 °C
Melting temperatureDSC341 °C
Hot deformation temperature0.45MPa,UnannealedASTM D648>260 °C
Physical propertiesTest ConditionTest MethodTest Result
densityASTM D7921.50 g/cm³
Electrical performanceTest ConditionTest MethodTest Result
Dissipation factor1MHzASTM D1505E-03
Surface resistivityASTM D2571E+13 ohms
Volume resistivityASTM D2571E+15 ohms·cm
Dielectric strengthASTM D14916 kV/mm
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.