Technical Data Sheet
Cured Properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Hardness (Shore) | 14to80 | ||
tensile strength | 4.65to10.6 MPa | ||
elongation at break | 700to1500 % | ||
tear strength | 24.5to52.5 kN/m |
Uncured Properties | Test Condition | Test Method | Test Result |
---|---|---|---|
density | 1.09to1.21 g/cm³ | ||
STORAGE STABILITY | 90to330 min |
Mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
tensile strength | ASTM D638 | 0.241to4.14 MPa |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.