Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|
density | | ASTMD792 | 1.10 g/cm³ |
Water absorption rate | | ASTMD570 | 0.30 % |
Water absorption rate | Saturation | ASTMD570 | 4.0 % |
hardness | Test Condition | Test Method | Test Result |
---|
| | ASTMD2240 | 81 |
Impact resistance | Test Condition | Test Method | Test Result |
---|
Impact strength of cantilever beam gap | | ASTMD256 | 48 J/m |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
tensile strength | Yield | ASTMD638 | 60.0 MPa |
elongation | Yield | ASTMD638 | 25 % |
Flexural modulus | | ASTMD790 | 1970 MPa |
bending strength | Yield | ASTMD790 | 103 MPa |
shear strength | | ASTMD732 | 52.4 MPa |
Tensile modulus | | ASTMD638 | 1650 MPa |
Thermal performance | Test Condition | Test Method | Test Result |
---|
Continuous use temperature | | ASTMD794 | 98.9 °C |
melting temperature | | | 210 °C |
| | ASTMD696 | 7E-05 cm/cm/°C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.