PA6 TEKAMID™ TB120G33

0
  • Properties:
    Filler
    glass fiber reinforced material
    33%
    filler by weight
  • Usages:
    Application in the automotive field

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
densityASTM D7921.38 g/cm³
Shrinkage rateASTM D9550.40to0.90 %
Water absorption rateASTM D5701.1 %
flammabilityTest ConditionTest MethodTest Result
UL flame retardant ratingUL 94HB
Mechanical propertiesTest ConditionTest MethodTest Result
elongationBreakASTM D6383.0 %
Flexural modulusASTM D7908340 MPa
bending strengthASTM D790235 MPa
tensile strength BreakASTM D638177 MPa
Impact resistanceTest ConditionTest MethodTest Result
Impact strength of cantilever beam gapASTM D256130 J/m
Thermal performanceTest ConditionTest MethodTest Result
Heat distortion temperatureASTM D648210 °C
melting temperatureASTM D3418220 °C
Heat distortion temperatureASTM D648220 °C
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.