PUR-Ester Andur 700-AP

0

Technical Data Sheet

thermosettingTest ConditionTest MethodTest Result
Thermosetting mixed viscosityASTMD23936400 cP
stripping time240 min
STORAGE STABILITY10到13 min
physical property Test ConditionTest MethodTest Result
Apparent densityASTMD18951.13 g/cm³
Shrinkage rateASTMD9551.0 %
hardnessTest ConditionTest MethodTest Result
Shore AASTMD224070
Mechanical propertiesTest ConditionTest MethodTest Result
tensile strengthYieldASTMD63822.1 MPa
elongationYieldASTMD638880 %
elastomerTest ConditionTest MethodTest Result
Tensile stressASTMD4121.54 MPa
Tensile stressASTMD4122.04 MPa
Tensile stressASTMD4122.56 MPa
compression setASTMD39523 %
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.