PP Homopolymer HIPOLEN P® EH 71 Hipol a.d.
0
Technical Data Sheet
| impact performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Impact strength of cantilever beam gap | 23°C | ISO 180 | 5.5 kJ/m² |
| mechanical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Bending modulus | ISO 178 | 1350 MPa | |
| tensile strength | Yield | ISO 527-2 | 34.0 MPa |
| Physical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| melt mass-flow rate | 230°C/2.16kg | ISO 1133 | 1.1 g/10min |
| density | ISO 1183/D | 0.900 g/cm³ |
| aging | Test Condition | Test Method | Test Result |
|---|---|---|---|
| AcceleratedOvenAging-air circuit | 150°C | Internal Method | 1.4 month |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.