Share
Add to compare

PA6 K225-KWS DSM Additive Manufacturing

Product Description
Certificates(0)
Datasheet

Product Description

Certificates

No Data...

Technical Data Sheet

impact performanceTest ConditionTest MethodTest ResultTest Unit
Impact strength of simply supported beam without notch23°CISO 179/1eU60kJ/m²
Impact strength of simply supported beam without notch-30°CISO 179/1eU55kJ/m²
Charpy Notched Impact Strength23°CISO 179/1eA6.0kJ/m²
Charpy Notched Impact Strength-30°CISO 179/1eA5.0kJ/m²
flammabilityTest ConditionTest MethodTest ResultTest Unit
UL flame retardant rating1.5mmIEC 60695-11-10,-20V-0
UL flame retardant rating0.38mmIEC 60695-11-10,-20V-0
mechanical propertiesTest ConditionTest MethodTest ResultTest Unit
Tensile strainYieldISO 527-23.5%
tensile strengthYieldISO 527-280.0MPa
Tensile modulusISO 527-23800MPa
Nominal tensile fracture strainISO 527-28.0%
thermal performanceTest ConditionTest MethodTest ResultTest Unit
Linear coefficient of thermal expansionTDISO 11359-29E-05cm/cm/°C
Linear coefficient of thermal expansionMDISO 11359-29E-05cm/cm/°C
Melting temperatureISO 11357-3220°C
Hot deformation temperature1.8MPa,UnannealedISO 75-2/A80.0°C
Hot deformation temperature0.45MPa,UnannealedISO 75-2/B200°C
Physical propertiesTest ConditionTest MethodTest ResultTest Unit
Water absorption rateEquilibrium,23°C,50%RHISO 622.5%
Water absorption rateSaturation,23°CISO 629.0%
Shrinkage rateTDISO 294-41.0%
densityISO 11831.18g/cm³
Electrical performanceTest ConditionTest MethodTest ResultTest Unit
Dissipation factor1MHzIEC 602500.020
Dissipation factor100HzIEC 602509E-03
Relative permittivity1MHzIEC 602503.20
Relative permittivity100HzIEC 602503.30
Dielectric strengthIEC 60243-130kV/mm
Volume resistivityIEC 600931E+15ohms·cm
Surface resistivityIEC 60093--ohms
Compared to the anti leakage trace indexIEC 60112V
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.