TPV Santoprene™ 701-80
28
- Properties:Dimensional stabilityOzone resistantRecyclableLow tendernessOil resistant
- Usages:Industrial applicationsAutomotive ApplicationsApplication in the automotive field
Technical Data Sheet
hardness | Test Condition | Test Method | Test Result |
---|---|---|---|
ISO868 | 83 |
elastomer | Test Condition | Test Method | Test Result |
---|---|---|---|
TearStrength-AcrossFlow3 | ISO34-1 | 30 kN/m | |
CompressionSet4 | ASTMD395B | 30 % | |
ASTMD395B | 47 % | ||
Compression permanent deformation 4 | ISO815 | 30 % | |
ISO815 | 47 % | ||
Tensile stress transverse flow rate | ASTMD412 | 5.20 Mpa | |
ISO37 | 5.20 Mpa | ||
Tensile strength - transverse flow rate | ASTMD412 | 8.80 Mpa | |
tensile strength | ISO37 | 8.80 Mpa | |
ASTMD412 | 290 % | ||
ISO37 | 290 % | ||
ASTMD624 | 30.0 kN/m |
aging | Test Condition | Test Method | Test Result |
---|---|---|---|
The rate of change in tensile strength in air | ASTMD573 | 6.0 % | |
ISO188 | 6.0 % | ||
ChangeinUltimateElongationAir | ASTMD573 | -37 % | |
ChangeinDurometerHardnessAir | ASTMD573 | 2.0 | |
ChangeinShoreHardnessinAir | ISO188 | 2.0 | |
Change rate of tensile strength | ASTMD471 | -38 % | |
ChangeinTensileStress | ISO1817 | -38 % | |
ChangeinUltimateElongation | ASTMD471 | -48 % | |
ChangeinTensileStrainatBreak | ISO1817 | -48 % | |
volume change | ASTMD471 | 4.0 % | |
ISO1817 | 4.0 % |
Thermal performance | Test Condition | Test Method | Test Result |
---|---|---|---|
brittle temperature | ASTMD746 | -32.0 °C | |
ISO812 | -32.0 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.