Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|---|---|---|
density | ISO2781 | 0.940 g/cm³ | |
Apparent density | ASTMD1895B | 0.40 g/cm³ | |
melt mass-flow rate | ISO1133 | 3.5到6.5 g/10min | |
AntioxidantAdditive | 内部方法 | >0.15 % | |
PolystyreneContent | 内部方法 | 29到31 % | |
TotalExtractables | 内部方法 | <1.0 % | |
Ash Content | ISO247 | 0.10到0.40 % | |
内部方法 | 4.0到6.0 % | ||
Volatile compounds | 内部方法 | <0.30 % | |
Solution viscosity- | 内部方法 | 1.3到1.9 Pa·s |
hardness | Test Condition | Test Method | Test Result |
---|---|---|---|
ASTMD2240 | 70 |
elastomer | Test Condition | Test Method | Test Result |
---|---|---|---|
Tensile stress | ISO37 | 2.90 MPa | |
tensile strength | Yield | ISO37 | 28.0 MPa |
elongation | Break | ISO37 | 800 % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.