physical property | Test Condition | Test Method | Test Result |
---|
Water absorption rate | | ISO62 | 0.36 % |
density | | ISO1183/A | 1.17到1.21 g/cm³ |
melt mass-flow rate | | ISO1133 | 15到22 g/10min |
Water absorption rate | | ISO62 | 0.15 % |
flammability | Test Condition | Test Method | Test Result |
---|
UL flame retardant rating | | UL94 | V-2 |
Burning wire flammability index | | IEC60695-2-12 | 850 °C |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
Tensile modulus | | ISO527-2/1A/1 | 2500到3000 MPa |
Tensile stress | Yield | ISO527-2/1A/50 | 60.0到70.0 MPa |
Tensile stress | Break | ISO527-2/1A/50 | 45.0到55.0 MPa |
Tensile strain | Yield | ISO527-2/1A/50 | 7.0到12 % |
Tensile strain | Break | ISO527-2/1A/50 | 25到30 % |
Flexural modulus | | ISO178 | 2000到2500 MPa |
Bending stress | | ISO178 | 55.0到65.0 MPa |
Impact resistance | Test Condition | Test Method | Test Result |
---|
Impact strength of simply supported beam without notch | | ISO179/1eU | 无断裂 |
Impact strength of cantilever beam gap | | ASTMD256 | 无断裂 |
| | ISO180 | 无断裂 |
Thermal performance | Test Condition | Test Method | Test Result |
---|
| | ASTMD648 | 125到135 °C |
Glass Transition Temperature | | 内部方法 | 140到150 °C |
vicat | | ISO306/A120 | 135到145 °C |
vicat | | ISO306/B120 | 130到140 °C |
| | ASTMD648 | 130到140 °C |
| | ISO75-2/B | 135到145 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.