PPS+PPE XYRON™ DG235 ASAHI JAPAN

0
  • Properties:
    Filler
    glass fiber reinforced material
    30%
    filler by weight

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
Shrinkage rate内部方法0.20to0.50 %
densityISO 11831.44 g/cm³
flammabilityTest ConditionTest MethodTest Result
UL flame retardant ratingUL 94V-1
Mechanical propertiesTest ConditionTest MethodTest Result
tensile strength ISO 527-2125 MPa
Tensile strainISO 527-22.0 %
Flexural modulusISO 1789750 MPa
bending strengthISO 178192 MPa
Impact resistanceTest ConditionTest MethodTest Result
Charpy Notched Impact StrengthISO 1797.0 kJ/m²
Electrical performanceTest ConditionTest MethodTest Result
Dissipation FactorIEC 602502E-03
Surface ResistivityIEC 600931E+16 ohms
Volume resistivityIEC 600931E+16 ohms·cm
dielectric constantIEC 602504.00
dielectric constantIEC 602504.00
Dissipation FactorIEC 602501E-03
Thermal performanceTest ConditionTest MethodTest Result
Heat distortion temperatureISO 75-2/A240 °C
Linear coefficient of thermal expansionISO 11359-23.5E-05 cm/cm/°C
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.