Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|---|---|---|
density | ASTMD1505 | 0.905 g/cm³ | |
melt mass-flow rate | ASTMD1238 | 0.75 g/10min |
film | Test Condition | Test Method | Test Result |
---|---|---|---|
Secant modulus | ASTMD882 | 600 MPa | |
tensile strength | ASTMD882 | 26.2 MPa | |
ASTMD882 | 24.8 MPa | ||
ASTMD882 | 58.6 MPa | ||
ASTMD882 | 37.9 MPa | ||
elongation | ASTMD882 | 750 % | |
ASTMD882 | 770 % | ||
Falling hammer impact | Blown Film | ASTMD1709A | 350 g |
Elmondov tear strength | ASTMD1922 | 55 g | |
ASTMD1922 | 300 g | ||
oxygen permeability | ASTMD3985 | 53 cm³·mm/m²/atm/24hr | |
Water vapor permeability | ASTMF1249 | 0.18 g·mm/m²/atm/24hr | |
Secant modulus | ASTMD882 | 689 MPa |
Thermal performance | Test Condition | Test Method | Test Result |
---|---|---|---|
melting temperature | DSC | 160到165 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.