Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|---|---|---|
density | 0.936 cm³/g | ||
Shrinkage rate | ASTMD2566 | 0.20 % | |
density | ASTMD792 | 1.04 g/cm³ | |
1.06 g/cm³ | |||
1.09 g/cm³ |
thermosetting | Test Condition | Test Method | Test Result |
---|---|---|---|
Thermosetting mixed viscosity | ASTMD2393 | 25.0 min | |
ASTMD2393 | 20.0 min | ||
ASTMD2393 | 240到360 min | ||
ASTMD2393 | 120到170 hr | ||
按重量计算的混合比:100,按容量计算的混合比:100 | |||
按重量计算的混合比:50,按容量计算的混合比:49 | |||
Shelf Life | 26 wk | ||
Thermosetting mixed viscosity | ASTMD2393 | 2100 cP | |
ASTMD2393 | 6000 cP | ||
ASTMD2393 | 60.0 cP |
hardness | Test Condition | Test Method | Test Result |
---|---|---|---|
Shore A | ASTMD2240 | 75到85 |
Supplementary Information | Test Condition | Test Method | Test Result |
---|---|---|---|
WeightGain | 3.7 % |
Mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Tensile modulus | ASTMD412 | 30.2 MPa |
elastomer | Test Condition | Test Method | Test Result |
---|---|---|---|
Tensile stress | ASTMD412 | 4.07 MPa | |
ASTMD412 | 5.17 MPa | ||
ASTMD412 | 6.21 MPa | ||
tensile strength | Yield | ASTMD412 | 10.2 MPa |
elongation | Break | ASTMD412 | 720 % |
tear strength | ASTMD624 | 39.4 kN/m |
Electrical performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Surface Resistivity | ASTMD257 | 5E+15 ohms | |
dielectric constant | ASTMD150 | 3.90 | |
Dissipation Factor | ASTMD150 | 0.010 | |
InsulationResistance | 3E+12 ohms |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.