TPV Alloy Elastoprene 70A-4000 KMI Group, Inc.

0

Technical Data Sheet

elastomerTest ConditionTest MethodTest Result
Permanent compression deformation125°C,70hrASTM D39545 %
tear strength23°CASTM D62440.0 kN/m
Permanent compression deformation70°C,22hrASTM D39529 %
elongationBreak,23°CASTM D412520 %
tensile strength100%Strain,23°CASTM D4123.30 MPa
tensile strengthYield,23°CASTM D4128.50 MPa
thermal performanceTest ConditionTest MethodTest Result
Brittle temperatureASTM D746-70.0 °C
Melting temperature159 °C
Physical propertiesTest ConditionTest MethodTest Result
densityASTM D7920.940 g/cm³
hardnessTest ConditionTest MethodTest Result
Shore hardnessShoreA,5SecASTM D224073
Shore hardnessShoreA,15SecASTM D224070
Supplementary InformationTest ConditionTest MethodTest Result
ozone resistanceASTM D1149Excellent
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.