PPE XYRON™  L543Z A1A3301 ASAHI JAPAN

106
  • Properties:
    Filler: Filler
    30% filler by weight

Technical Data Sheet

物理性能Test ConditionTest MethodTest Result
收缩率2.00mm内部方法0.20to0.45 %
吸水率23°C,24hrISO620.060 %
室外适用性BlackUL746Cf1
热性能Test ConditionTest MethodTest Result
热变形温度1.8MPa,未退火ASTMD648120 °C
热变形温度1.8MPa,未退火ISO75-2/A118 °C
线性热膨胀系数MD:-30到65°CISO11359-24E-05 cm/cm/°C
可燃性Test ConditionTest MethodTest Result
UL阻燃等级0.40mmUL94HB
UL阻燃等级0.75mmUL94V-1
机械性能Test ConditionTest MethodTest Result
拉伸应力屈服,23°CISO527-280.0 Mpa
拉伸应变断裂,23°CISO527-22.0 %
弯曲模量23°CISO1787060 Mpa
弯曲应力23°CISO178138 Mpa
电气性能Test ConditionTest MethodTest Result
介电常数1MHzIEC602503.20
耗散因数100HzIEC602506E-03
耗散因数1MHzIEC602508E-03
表面电阻率IEC600931E+16 ohms
体积电阻率23°CIEC600931E+16 ohms·cm
介电常数100HzIEC602503.30
冲击性能Test ConditionTest MethodTest Result
简支梁缺口冲击强度323°CISO1795.0 kJ/m²
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.