PP K-Prene XL-A40 Technovinyl Polymers India Ltd.

0

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
densityASTM D7920.990 g/cm³
hardnessTest ConditionTest MethodTest Result
Shore hardnessShore AASTM D224040
Supplementary InformationTest ConditionTest MethodTest Result
ozone resistancePass
elastomerTest ConditionTest MethodTest Result
Stretch permanent deformationASTM D41210 %
elongationBreakASTM D412600 %
tear strengthASTM D62415.0 kN/m
compression setASTM D39535 %
compression setASTM D39545 %
tensile strength ASTM D4121.00 MPa
tensile strength ASTM D4121.50 MPa
tensile strength YieldASTM D4123.20 MPa
Thermal performanceTest ConditionTest MethodTest Result
brittle temperatureASTM D746<-60.0 °C
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.