PP INSPIRE™ 227

0

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
densityASTMD7920.900 g/cm³
melt mass-flow rateASTMD12383.2 g/10min
optical performance Test ConditionTest MethodTest Result
glossASTMD245732
Haze ratioASTMD100323 %
filmTest ConditionTest MethodTest Result
Secant modulusASTMD8821170 MPa
Secant modulusASTMD8821140 MPa
Falling hammer impactASTMD1709A50 g
Elmondov tear strengthASTMD192214 g
Elmondov tear strengthASTMD192224 g
tensile strengthASTMD88227.0 MPa
tensile strengthASTMD88241.0 MPa
tensile strengthASTMD88238.0 MPa
tensile strengthASTMD88239.0 MPa
elongationASTMD882250 %
elongationASTMD8826.0 %
Film thickness - tested50 µm
ASTMD57480.500 J
ASTMD574842.0 N
Thermal performanceTest ConditionTest MethodTest Result
内部方法162到166 °C
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.