Share
Add to Compare

TPV 8211-55 CELANESE USA

168

Form:Granules | Grade:Weather resistant grade

Properties:
dimensional stability Low friction coefficientRecyclable materialsCleanableGood forming performanceGood colorabilityHigh mobilityOzone resistanceChemical resistancesoftLow water absorptionNot absorbing water
Typical Applications:
packingAutomotive sectorSoft handleSmart phoneConsumer goods sectorConsumer product application fieldpackingSoft handlePhoneApplication in the automotive field
Product Description
Certificates(0)
Datasheet

Product Description

Typical Applications:packing | Automotive sector | Soft handle | Smart phone | Consumer goods sector | Consumer product application field | packing | Soft handle | Phone | Application in the automotive field
Properties:dimensional stability | Low friction coefficient | Recyclable materials | Cleanable | Good forming performance | Good colorability | High mobility | Ozone resistance | Chemical resistance | soft | Low water absorption | Not absorbing water

Certificates

No Data...

Technical Data Sheet

flammabilityTest ConditionTest MethodTest ResultTest Unit
UL flame retardant rating3.0mmUL 94HB
UL flame retardant rating1.1mmUL 94HB
elastomerTest ConditionTest MethodTest ResultTest Unit
Permanent compression deformation125°C,70hr4ISO 81549%
Permanent compression deformation70°C,22hr4ISO 81519%
Permanent compression deformation125°C,70hr3ASTM D395B49%
Permanent compression deformation70°C,22hr3ASTM D395B19%
elongationBreak,23°C,Across FlowASTMD412480%
tensile strengthBreak,23°C,横向FlowASTMD4124.60Mpa
Tensile stress100%Strain,23°C,横向FlowASTMD4122.10Mpa
thermal performanceTest ConditionTest MethodTest ResultTest Unit
Brittle temperatureASTMD746-62.0°C
RTI3.0mmUL 74695.0°C
RTI1.1mmUL 74690.0°C
RTI ElecUL 746100°C
hardnessTest ConditionTest MethodTest ResultTest Unit
Shore hardnessShoreA,15Sec,23°CISO 86859
agingTest ConditionTest MethodTest ResultTest Unit
Change rate of hardness (Shore) in the airShoreA,150°C,168hrASTMD5731.0
Change rate of ultimate elongation in air150°C,168hrASTMD573-10%
Change rate of tensile strength in air150°C,168hrASTMD573-11%
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.