ABS DENIBLEND H

0

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
densityASTMD7921.16 g/cm³
Water absorption rateSaturationASTMD5700.15 %
Mechanical propertiesTest ConditionTest MethodTest Result
Tensile modulusASTMD6382200 MPa
tensile strengthYieldASTMD63850.0 MPa
elongationBreakASTMD638>100 %
Impact resistanceTest ConditionTest MethodTest Result
Impact strength of cantilever beam gapISO180/A50 kJ/m²
ISO180无断裂
Thermal performanceTest ConditionTest MethodTest Result
RTI ElecUL74680.0 °C
RTI ImpUL74680.0 °C
RTIUL74680.0 °C
ASTMD648A115 °C
vicatASTMD15252140 °C
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.