Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|
Shrinkage rate | | ASTM | 0.5-1.0 % |
other | Test Condition | Test Method | Test Result |
---|
| | | 20%玻璃纤维增强,高刚性,低收缩,高机械强度 |
purpose | | | 控制器外壳,家电产品等。 |
Basic performance | Test Condition | Test Method | Test Result |
---|
melt mass-flow rate | | ASTM D-1238 | 4.0 g/10min |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
| | ASTM D-790 | 35000 kg/cm2 |
Notch impact strength | | ASTM D-256 | 7 kg.cm/cm |
Tensile strength (drop point) | | ASTM D-638 | 800 kg/cm2 |
Rockwell hardness | | ASTM D785 | 105 |
Electrical performance | Test Condition | Test Method | Test Result |
---|
dielectric breakdown strength | | ASTM D-149 | 40 KV/mm |
Physical properties | Test Condition | Test Method | Test Result |
---|
density | | ASTM D792/ISO 1183 | 0.9 |
Thermal performance | Test Condition | Test Method | Test Result |
---|
| | ASTM D-648 | 160 °C |
| | ASTM D648/ISO 75 | 110 ℃(℉) |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.