Technical Data Sheet
thermosetting | Test Condition | Test Method | Test Result |
---|
| Resin | | 按重量计算的混合比:100按容量计算的混合比:4.7 |
| Hardener | | 按重量计算的混合比:19按容量计算的混合比:1.0 |
| | | 33 min |
Thermosetting mixed viscosity | | ASTMD2393 | 475 cP |
stripping time | | | 2900 min |
physical property | Test Condition | Test Method | Test Result |
---|
Apparent density | | ASTMD1895 | 1.09 g/cm³ |
Shrinkage rate | | ASTMD955 | 0.020 % |
Water absorption rate | | ASTMD570 | 0.30 % |
hardness | Test Condition | Test Method | Test Result |
---|
| | ASTMD2240 | 75 |
Mechanical properties | Test Condition | Test Method | Test Result |
---|
Tensile modulus | | ASTMD638 | 20500 MPa |
tensile strength | Break | ASTMD638 | 241 MPa |
elongation | Yield | ASTMD638 | 11 % |
Flexural modulus | | ASTMD790 | 9720 MPa |
compressive strength | | ASTMD695 | 29.5 MPa |
Thermal performance | Test Condition | Test Method | Test Result |
---|
| | ASTMD648 | 52.2 °C |
| | ASTMD696 | 6.9E-05 cm/cm/°C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.