Technical Data Sheet
thermosetting | Test Condition | Test Method | Test Result |
---|---|---|---|
按重量计算的混合比:1.0 | |||
按重量计算的混合比:1.0 | |||
Shelf Life | 52 wk |
Uncured Properties | Test Condition | Test Method | Test Result |
---|---|---|---|
DIN53019 | 7.0到9.5 Pa·s | ||
Curing Time | 0.17到0.25 hr |
hardness | Test Condition | Test Method | Test Result |
---|---|---|---|
Shore A | ASTMD2240 | 8到10 |
elastomer | Test Condition | Test Method | Test Result |
---|---|---|---|
tensile strength | ASTMD412 | >2.50 MPa | |
elongation | Break | ASTMD412 | >500 % |
tear strength | ASTMD624 | >3.00 kN/m | |
compression set | DIN53517 | 25 % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.