HDPE HWB-1051

0

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
melt mass-flow rateASTMD123810 g/10min
Resistance to environmental stress crackingASTMD1693>1000 hr
Resistance to environmental stress crackingASTMD1693B150 hr
densityASTMD15050.951 g/cm³
melt mass-flow rateASTMD12380.060 g/10min
Supplementary InformationTest ConditionTest MethodTest Result
Blow molding temperature190到210 °C
Mechanical propertiesTest ConditionTest MethodTest Result
tensile strengthASTMD63824.8 MPa
elongationASTMD638800 %
Flexural modulusCompression MoldedASTMD7901070 MPa
Impact resistanceTest ConditionTest MethodTest Result
Tensile impact strengthCompression MoldedASTMD1822347 kJ/m²
Thermal performanceTest ConditionTest MethodTest Result
brittle temperatureASTMD746<-90.0 °C
ASTMD64844.0 °C
vicatASTMD1525129 °C
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.