TPV Santoprene™ 8191-75B500
4
- Properties:Chemical resistanceFlame retardant
- Usages:Profilebuilding materialsKitchen utensilsParts under the hood of a carMovable hingeMirror frameAdhesive resinSoft handleConsumer product application fieldFatigue relief suppliesPhoneBondingApplication in the automotive fieldsporting goodsLarge and small household appliancesHome appliance componentspackingElectrical appliances
Technical Data Sheet
hardness | Test Condition | Test Method | Test Result |
---|---|---|---|
ISO868 | 53 |
flammability | Test Condition | Test Method | Test Result |
---|---|---|---|
UL flame retardant rating | UL94 | HB | |
UL94 | HB |
elastomer | Test Condition | Test Method | Test Result |
---|---|---|---|
ASTMD412 | 600 % | ||
ISO37 | 600 % | ||
CompressionSet2 | ASTMD395B | 55 % | |
CompressionSet3 | ISO815 | 55 % |
aging | Test Condition | Test Method | Test Result |
---|---|---|---|
Change rate of tensile strength in air | ASTMD573 | -28 % | |
ASTMD573 | -61 % | ||
ISO188 | -28 % | ||
ISO188 | -61 % | ||
Change rate of hardness of hardness tester 2 | ASTMD471 | -33 | |
ASTMD471 | 4.0 | ||
ASTMD471 | 5.0 | ||
ChangeinShoreHardness | ISO1817 | 2.0 | |
ISO1817 | 4.0 | ||
ISO1817 | -33 | ||
ISO1817 | 4.0 | ||
ISO1817 | 5.0 | ||
Change rate of ultimate elongation in air | ASTMD573 | -14 % | |
ASTMD573 | -70 % | ||
Changes in tensile stress during fracture in air | ISO188 | -14 % | |
ISO188 | -70 % | ||
The rate of change in hardness of an air hardness tester | ASTMD573 | -4.0 | |
ASTMD573 | 8.0 | ||
Change rate of Shore hardness in air | ISO188 | -4.0 | |
ISO188 | 8.0 | ||
Change rate of tensile strength | ASTMD471 | -17 % | |
ASTMD471 | -1.0 % | ||
Change rate of ultimate elongation | ASTMD471 | -68 % | |
ASTMD471 | -7.0 % | ||
ASTMD471 | -12 % | ||
Changes in tensile stress during fracture | ISO1817 | -3.0 % | |
ISO1817 | -9.0 % | ||
ISO1817 | -68 % | ||
ISO1817 | -7.0 % | ||
ISO1817 | -12 % | ||
Change rate of hardness of hardness tester 2 | ASTMD471 | 2.0 | |
ASTMD471 | 4.0 | ||
Change rate of tensile strength | ASTMD471 | -85 % | |
ASTMD471 | 1.0 % | ||
ASTMD471 | 2.0 % | ||
ISO1817 | -17 % | ||
ISO1817 | -1.0 % | ||
ISO1817 | -85 % | ||
ISO1817 | 1.0 % | ||
ISO1817 | 2.0 % | ||
Change rate of ultimate elongation | ASTMD471 | -3.0 % | |
ASTMD471 | -9.0 % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.