LDPE DFD-4960 STYRON US
2
- Properties:Electrical performance
Technical Data Sheet
| machinability | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Melt Temperature | 138-160 °C |
| Basic Performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| melt mass-flow rate | 190℃/2.16kg | ASTM D-1238 | 2.1 g/10min |
| density | ASTM D-792 | 0.918 g/m |
| mechanical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Elongation at Break | ASTM D-638 | 500 % | |
| tensile strength | ASTM D-638 | 11.4 Mpa |
| Electrical performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Dissipation factor | 1E+6Hz | ASTM D-150 | 0.0003 |
| Dielectric constant | 1E+6Hz | ASTM D-150 | 2.28 |
| Dielectric strength | 3.18mm | ASTM D-149 | 8.66 KV/mm |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.