HDPE LH-402

0
  • Usages:
    Pipeline system

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
Resistance to environmental stress crackingASTMD1693B>3000 hr
melt mass-flow rateASTMD12380.62 g/10min
densityASTMD15050.944 g/cm³
melt mass-flow rateASTMD12380.14 g/10min
Supplementary InformationTest ConditionTest MethodTest Result
PipePropertiesISO1167>1 yr
PipePropertiesISO1167>1 yr
PipePropertiesISO1167>1 yr
Mechanical propertiesTest ConditionTest MethodTest Result
tensile strengthYieldASTMD63822.6 MPa
elongationBreakASTMD638>600 %
Flexural modulusASTMD790785 MPa
Impact resistanceTest ConditionTest MethodTest Result
Impact strength of cantilever beam gapASTMD256NoBreak
Thermal performanceTest ConditionTest MethodTest Result
OxidationInductionTimeASTMD3895>40 min
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.