Polyester Alloy

Polyester Alloy Vipel® F764-BBD-00

0

Technical Data Sheet

Uncured PropertiesTest ConditionTest MethodTest Result
density1.09 g/cm³
0.40 Pa·s
GelTime20 min
physical property Test ConditionTest MethodTest Result
StyreneContent42 %
hardnessTest ConditionTest MethodTest Result
Barcol HardnessASTMD258351
Supplementary InformationTest ConditionTest MethodTest Result
GeltoPeak10.0 min
PeakExotherm212 °C
Mechanical propertiesTest ConditionTest MethodTest Result
bending strengthASTMD790123 MPa
Tensile modulusASTMD6383520 MPa
tensile strengthASTMD63869.6 MPa
elongationBreakASTMD6382.3 %
Flexural modulusASTMD7903860 MPa
Thermal performanceTest ConditionTest MethodTest Result
ASTMD648139 °C
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.