Basic performance | Test Condition | Test Method | Test Result |
---|---|---|---|
density | ASTM D-4025 | 0.928 g/cm | |
styrene content | Internal Method | % | |
Total extraction rate | Internal Method | <1.0 % | |
Volatile compounds | Internal Method | <0.5 % |
Mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
tensile strength | ASTM D-412 | 1.10 MPa | |
elongation | ASTM D-412 | 1000 % |
Other performance | Test Condition | Test Method | Test Result |
---|---|---|---|
Antioxidant additive | Internal Method | % | |
Dust content | Internal Method | % |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.