TPV Supersoft Actymer® AE-2000S

0

Technical Data Sheet

physical property Test ConditionTest MethodTest Result
densityISO 11830.918 g/cm³
hardnessTest ConditionTest MethodTest Result
Shore hardnessISO 8683
elastomerTest ConditionTest MethodTest Result
tensile strength ISO 370.100 MPa
tensile strength YieldISO 371.70 MPa
elongationBreakISO 37830 %
tear strengthISO 34-18.0 kN/m
compression setISO 81528 %
compression setISO 81564 %
agingTest ConditionTest MethodTest Result
Change rate of tensile strength in airISO 188-10 %
Tensile stress change rateISO 188-20 %
Thermal performanceTest ConditionTest MethodTest Result
brittle temperatureISO 974-60.0 °C
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.