ABS XR-409H CNOOC&LG HUIZHOU
40
- Properties:heat-resistingHigh mobilityHigh rigidity
- Usages:Automotive sectorHome appliance components
Technical Data Sheet
| Other performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Compared to the anti leakage trace index | UL -746A | PLCCode |
| mechanical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| tensile strength | ASTM D-638 | 500 kg/cm | |
| Elongation at Break | ASTM D-638 | 20 % | |
| Bending modulus | ASTM D-790 | 820 kg/cm | |
| Rockwell hardness | R-Scale | ASTM D-785 | 107 |
| Bending modulus | ASTM D-790 | 24000 kg/cm | |
| impact elasticity | Notched1/4" | ASTM D-256 | 11 kgcm/cm |
| thermal performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Hot deformation temperature | Unannealed18.5kg/cm2,1/2" | ASTM D-648 | 113 °C |
| Vicat softening temperature | 1.000g | ASTM D-1525 | 137 °C |
| Burning rate | 1/8" | UL -94 | HB |
| 1/8" | IEC 707 | FH3-34 mm/min | |
| 1/16" | UL -94 | HB |
| Physical properties | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Shrinkage rate | ASTM D-955 | 0.003-0.005 mm/mm | |
| melt mass-flow rate | 220℃/10kg | ASTM D-1238 | 4 g/10min |
| Electrical performance | Test Condition | Test Method | Test Result |
|---|---|---|---|
| Hot wire ignition | UL -746A | PLC 5 | |
| High arc combustion index | UL -746A | PLC 0 | |
| High voltage arc tracing rate | UL -746A | PLC 2 | |
| Arc resistance | ASTM D-495 | PLC_6 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.