Technical Data Sheet
physical property | Test Condition | Test Method | Test Result |
---|---|---|---|
Flame Fusion Index | JIS K6922 | 3.5 g/10min | |
Environmental stress cracking resistance constant load method | JIS K6922 | 1000 hr |
hardness | Test Condition | Test Method | Test Result |
---|---|---|---|
Shore hardness D | JISK7215 | 42 |
Mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
JIS K6922 | 500 % | ||
Flexural modulus | JIS K6922 | 56 Mpa | |
Impact of simply supported beam gap | JIS K6922 | NB kJ/m² |
Thermal performance | Test Condition | Test Method | Test Result |
---|---|---|---|
vicat | JIS K7206 | 72 °C | |
JIS K7121 | 90 °C | ||
brittle temperature | ISO 974 | -70 °C |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.