Technical Data Sheet
thermosetting | Test Condition | Test Method | Test Result |
---|---|---|---|
Thermosetting mixed viscosity | Brookfield | 15.0 cP | |
Brookfield | 1240 cP | ||
Brookfield | 170 cP | ||
Brookfield | 480到720 min | ||
按重量计算的混合比:50,按容量计算的混合比:47 | |||
按重量计算的混合比:100,按容量计算的混合比:100 | |||
Shelf Life | 26 wk | ||
Thermosetting mixed viscosity | Brookfield | 1050 cP | |
Brookfield | 20.0到25.0 min | ||
Brookfield | 15.0到20.0 min |
physical property | Test Condition | Test Method | Test Result |
---|---|---|---|
density | 1.09 g/cm³ | ||
ASTMD792 | 1.05 g/cm³ | ||
Contractility | ASTMD2566 | 0.20 % | |
density | 0.921 g/cm³ | ||
1.02 g/cm³ |
hardness | Test Condition | Test Method | Test Result |
---|---|---|---|
ASTMD2240 | 10到20 | ||
ASTMD2240 | 65到75 | ||
ASTMD2240 | 25到35 |
Supplementary Information | Test Condition | Test Method | Test Result |
---|---|---|---|
CureTime | 5.0到7.0 day |
Mechanical properties | Test Condition | Test Method | Test Result |
---|---|---|---|
Tensile modulus | ASTMD412 | 0.186 MPa |
elastomer | Test Condition | Test Method | Test Result |
---|---|---|---|
tensile strength | Yield | ASTMD412 | 3.90 MPa |
elongation | Break | ASTMD412 | 1300 % |
tear strength | ASTMD624 | 10.7 kN/m |
Electrical performance | Test Condition | Test Method | Test Result |
---|---|---|---|
dielectric constant | ASTMD150 | 6.61 | |
Dissipation Factor | ASTMD150 | 0.051 |
IMPORTANT NOTES: Plas.com collected the data in the data sheet from the material manufacturers. Plas.com makes the best effort to improve the accuracy of the data, but has no responsibility for the data. We strongly recommend verifying the validity of the data with the material manufacturers before making a final decision.